Results 1 to 10 of 12
Threaded View
-
02-12-2017, 11:15 AM #1
- Join Date
- Feb 2017
- Posts
- 4
Troubleshooting TPE w/ Powerspec I3 plus
New to 3D printing and I could use some advice on what my prints are trying to tell
me, the following is done is Cura.
First Print
- Print speed - 30mm/s
- Print temp. - 235°
- Bed temp. - 55°
- Initial layer thickness - 0.3
- Initial layer line width - 100
*Printer set to run it at 35% from there moved up to 55%. No advanced speed changes
Second Print
- Print speed - 15mm/s
- Travel speed - 15 mm/s
- Bottom layer speed - 15 mm/s (rest of advanced speeds set to 0 to match print speed)
- Print temp. - 235°
- Bed temp. - 55°
- Initial layer thickness - 0.3
- Initial layer line width - 100
*Flow increased by 5% (105%) resulted in a slightly better base. Yet still faulted when layering the ends of the dpad.
Last edited by SmoothVoltron; 02-12-2017 at 01:59 PM.
New member with print issue