At the higher temp, the filament flows better. That gives it more time to seep into the cracks of the tape.

But, did you try printing that first layer .1mm closer to the bed?

After 6 months, the printer has changed much also. Maybe not much but some.

If you REALLY wish to experience not sticking, switch to ABS...