06-14-2016, 05:28 AM #8
looks like across between pla and nylon.
so be wary of this if you plan to use an open flame to heat a clogged extruder with the stuff in it. I have lit the entire back side of an 30x1000mm extruder on fire before. Some brands have flame retardants in them, but even still the stuff will ignite.
You're mad. :-)