Just tripped over this forum. I've been printing with PLA on all of my printers without issue, but I cant get ABS to do anything right. What brand is working well for you all. I'm using gizmo dorks PLA and ABS, because the PLA I get from them is always perfect. I've tried up to 235 with my Solidoodle Workbench using E3d V6's, and I have to say I've melted a lot of useless plastic at this point. From the looks of things maybe I should go hotter. What kind of bed settings are you using? What are you using to keep things stuck down? I tried ABS juice, and it works well on my Prusa with hardware store garbage glass, but the workbench has borosilicate glass, which seems to laugh at it. I had ok luck with hairspray, but only with smaller jobs. Help!!!