Quote Originally Posted by Sebastian Finke View Post
I'm using 0.7% as the shrinkage factor.
Ah, thanks. I misread that. We actually calculated 1.15%, I think; but normally we just oversize the .stl by 1% in all axes. Perhaps because we usually print ABS at 235C.