Results 1 to 10 of 16
Threaded View
-
05-31-2015, 11:47 AM #3
Thanks.
Board is ready. Beautiful result. But measuring shows that the first centimeter has shrunk over all by 10% and some more on the edges where it curls up.
What i'll do now is
- print it laying down in stead of standing up (the board is 130x105x25).
- print the first layers with brim very slow (thanks for the advice).
- Then after 5mm i lower the temp of the glass plate to 30 degrees C.
Any more suggestions?