    hi!
    iam using 3.2mm glass now. did you guys increase temperature, coz the glass will eat some of the heat? by how much?
    my temp is already 120. using abs. some parts of object still lift. specially corners.
    already tried raft with 2 layers 6mm, it still lift. latest print 2 corner lift almost 4.5-5mm. 2 corner 0.5-1mm

    will try the acetone slurry next, but any suggestions will be appreciated.