I see I've ruffled some feathers... are you always so hostile?
Wasn't attacking you or anyone else. Reading the thread again you seem to value your personal experience over what F3D or anyone else knows. The link I provided is a good starting point if you're curious though.
Since you asked here's some specific examples:
The front bead should be pretty much just a flat strip
The bed heat needs to be at least 60c for pla and most other filaments - never go lower
print your pla at least at 205 - 210-215 is usually better
I tend to go back to 10% for the pet-g, whereas I can run the pla at 30% for the first layer.
And here's you (not) recommending only acetone twice:
Alcohol would work just as well I guessif it stays shiny - it's fine to use on the rest.
Some of this is admittedly nit-picky but it's good to remember that people (especially those new to 3d printing) will take what you say quite literally.
Holes and pockmarks in print walls