  1. #6
    Engineer
    Join Date
    Aug 2014
    Location
    Montreal, Quebec
    Posts
    576
    When they upgraded their new liner to this one, all I can see is a joke. That much plasticity deformation will eventually lead to printer's death.


    https://www.youtube.com/watch?v=UgALH8PcjQ4

    I am also currently designing my own vat for the pegasus touch, 75$ for pissed poor quality acrylic vat with plenty of stress concentration, was the reason that push me looking for a DIY version.

    I do not have much experience with pyrex glass, I don't know if you can use those silicone caulk for glass to glue them.

    I do have a big sheet of acrylic (3mm) that I planned to thermoform and shape box. Planning to use it for the vat, but I would prefer to go with glass, since it will be harder to scratch.

    Also for your silicone are you using the one from sylgard?