    If you get it working, it would probably burn out better than PLA, so metal casts will likely be cleaner. I don't see it being fine enough for jewelry or dentistry, but for simple functional parts it could work well.

    Andrew Werby
    Juxtamorph.com

  2. #2
    Technician
    Join Date
    Jan 2015
    Location
    Traverse City MI
    Posts
    53
    Add Wes@MachWax on Facebook
    Correct on both points. It will definitely burnout cleaner than PLA, and the detail would be sub par for most jewelers/dental labs. There is some minor interest for the smaller operations who may not have the money to buy the more expensive printers who would be willing to print, and modify by hand to suit the finer detail necessary with jewelry.