Originally Posted by
wirlybird
Here is a cube I am doing, trying to dial in some Hatchbox ABS. The pics are of the same spot on the cube from different angles.
ABS - 210
Bed 90
QIDI Tech-1 fully enclosed
S3D
This is the corner set for start points. I have been turning down the temp to see if this will go away or reduce but it is not.
I am ran a print with start point optimized to see how that did and that spot is better but still there.
Qidi X Plus 3 Paper thin first...