Quote Originally Posted by wirlybird View Post
Yes, that was with the red crystal straight out of the package. I am going to run a decreasing temp test to see where the stringing stops. That is what I did for the PLA and finally found 190 to be good. My concern is if I am getting a good bond at that temp.
The other thing I am questioning is if the extraction settings are even working on the left extruder. I can turn things way up and see no change in the print.

I am down to 190 for the Crystal Red print. Almost no stringing but a bit fragile compared to the same part in regular PLA. I wonder at what point adhesion or bonding starts to fail or not be good.
Pretty good looking print though. I'll post a pic on the next sample.