    BTW, I also use the Inland microcenter PLA and after printing a temp tower it seems to actually like 196 deg. the best. I run my bed at 50C but honestly you could probably go down on that too. If I have a big footprint print then sometimes w/ blue painters tape it's hard to get off but if I let it cool it's fairly easy after I break the bond at one corner. I found even going to 30C helped w/ the super adhesion of prints.

    Dave

  2. #2
    Interesting! I'd gone with the higher temps becuase that's what was indicated on the ackaging, but I'll give some lower temps a try too.