Close



Results 1 to 10 of 40

Threaded View

  1. #5
    Student
    Join Date
    Apr 2014
    Location
    Germany
    Posts
    10
    Add NitroXpress on Thingiverse
    Hi,

    230° is enough.
    Print perimeters outside-in.
    I have absolut no problems with stringing !

    PETG is a much better material than PLA.
    I only use PETG.
    PETG does not absorb water !
    I print PETG at 160mm/sec.
    No need to slowdown the print.

    High quality prints at 80mm/sec:

    lizzard.jpg
    Last edited by NitroXpress; 04-03-2016 at 12:18 PM.