Results 1 to 10 of 20
Hybrid View
-
07-27-2020, 10:06 AM #1
- Join Date
- May 2018
- Posts
- 566
abs breaks down in UV, or so they say.. you should look at PETG for this part if it is only heat/sun that is driving no PLA. The part looks simple without a lot of small projections. PETG would be perfect, I use it for outside camera mounts. No enclosure, not warping but not a ridge as ABS but very durable bends a lot before it breaks.
-
07-27-2020, 10:13 AM #2
- Join Date
- Jul 2020
- Posts
- 20
Please explain to me how to...