Results 1 to 10 of 13
Thread: Printing POM/Delrin...it sticks!
Threaded View
-
06-13-2016, 10:29 AM #2
You really need a hot build plate for this stuff. Like 130+. Then Extruder temps should be around 195 or 200. I haven't tried it but evidently a thick ABS slurry on Glass works.
Qidi X Plus 3 Paper thin first...
05-27-2024, 01:15 AM in General 3D Printing Discussion