I have a 1/4 in glass on top of the build plate with .05 mm heat sink tape under and no blue sticker. I found at only 110 I don't get the ABS to adhere will on the first or subsequent passes. So I upped the temp to 115 on the build plate. Seems to work with no hair spray. When the glass cools the print just falls off like butter.

Quote Originally Posted by DarkAlchemist View Post
Then why was I the lucky one? I mean I can't have been the only one with this issue but who knows.

Oh, are you printing at 110c as the blue "pc glue" says? btw, at 110c that blue "pc glue" turned brown (same color as that sticky back tape in the video on how to remove the stuff) and even the bottom of the print I did was brown.