    You think it is most likely caused by the manufacturing process or feed stock...
    Is this not a indicator for quality ?

    I have printed a wind turbine with PETG.
    And on the roof, is definitely a humid ambient.
    If PETG absorbs so much water over the time, it have to crack in the winter when become frosted, or ?