FYI:
I print PLA at 180-190 (depending on the overall size of the print) on a glass bed with hairspray as my 'glue'. Bed temp is 40, altho, I likely don't need it.
Could it be moisture in the filament, that is 'boiling-out' at the high temps?
Printer will print perfect...