I finally got prints coming out perfect with the PETG on the blue tape that comes with the flashforge, with it sticking well and removing easy. I set the temp for extruder to 240C and bed to 65C The only problem I still have is it still leaves semi-translucent glossy lines on the print tape from the first layer of the print and alcohol doesn't seem to clean it off. I haven't had any adhesion problems in that area and I printed several times on top of it so it doesn't seem to be ruining the tape yet or causing adhesion problems, but I am not sure if it will eventually. you can barely see the lines and its easier to see in low light at a certain angle. Not sure what to use to clean it.

I have some screenshots of the print bed and the prints that came out good after tweaking a few extra settings in S3D. I also set the z-offest to 0.2 so that the layers are not squished like with PLA and this stopped the stringing problem I was having and I also slowed down the print speed.

IMG_20151109_164858.jpg

IMG_20151109_165108.jpg