I hope it works.
Another option is to print the first few layers with the bed at 110C, then reduce the bed temp to 80-90C, so that there's not so much difference between the temperatures of the layers. I really think temperature difference is the cause of your issue. I print ABS with the bed at 70C the whole time - but with hair spray.