Yeah way too hot,
Run PLA at 200-205c
Hotbed at 65c
And Ghosty's right, more shells. When it prints shells or 'walls' it does them from the inside to the outside which makes the exterior wall more rigid.
Movement and Travel I would go anywhere from 50-60ms feed to 70ms feed, travel 100-120msHex3D - 3D Printing and Design http://www.hex3d.com