Please Post Images.
Probable Cause -filament adsorbed moisture.
Solution - Using a dehydrator
Type Temperature Glass Transition Duration PLA 122° F 140-150° F 8 Hours PETG 140° F 165-175° F 4 Hours ABS 158° F 220-230° F 4 Hours