I am using an Ender 3 Pro
My layer height is 0.3
My print temp is 210
My build plate temp is 60
My flow is 100
My retraction distance is 7 mm
My retraction speed is 50mm/s
My fan speed is 25
My Build plate adhesion type is skirt
My skirt line count is 4
I am printing on glass and I use pritt stick.
I use Cura to slice my files. This is happening with all the things I try and print. It also happened when I just tried to print a test file that came with the printer. I have enclosed a photo of the failed test file print.