This is what I would call normal for FFF .. It isn't injection molding..
Totally different printer and Simplified 3d slicer.. can I do a zhop to reduce this, yes but it will slow down my print and make for more blobs as it move the nozzle away from the surface allowing for more strings (filament dependent) and only matter on the last layer.. could probably do 2 process in S3D and hop on the last few layers but I have come to accept this as normal.
Good luck
Drag mark along with PETG pop drops.. :-)
nozzle drag.jpgLast edited by airscapes; 05-09-2019 at 11:00 AM.