I have found I have to treat the PLA/PHA like ABS temp wise. I am running it at 220 ext, 90 bed. Test print was ok.
The calibration test was done at 210 ext, and 70 bed. Slight warping. With the temps hotter it should help. I also put the front door back on but left the top open. It is rather cold in the room.
[IMG] [/IMG]