I'm sure this is a dead horse, but after making some decent prints in PLA, ABS seems to be dreadful. I have yet to make one stick. Specifically on the corners (I know, I said ends. I meant corners). I am using 110 for the bed temp, and 230 for the nozzle, although I've tried as high as 250 nozzle, since that's what came on the download from MakerFarm. Tried spraying the glass with hairspray, which did next-to-nothing, and also tried blue painter's tape, which made it stick for like 10 layers or so, before it gave up.

Any tips on making ABS stick? I'll try to find acetone to make some ABS juice. In the meantime, I had some things I wanted to print in ABS instead of PLA.

I'd also love to see configs for Slic3r and/or Cura (haven't had success at all in the latter). I'm running a .04 Hexagon. Stock fan shroud.

Thanks again, guys.