Hello curious aardvark! Thanks for replying!
Yeah, I'm printing via SD. I'm printing PLA at a (default) temperature of 220?C. I've read that this temperature might be too high - and it may be, as I believe some of the material leaks towards the end.
I too have read that those markings can be adjusted via the retraction settings. I've since adjusted some values since. This is my current setup:
- Initial Printing Temperature: 210?C
- Printing Temperature: 210?C
- Final Printing Temperature: 205?C
- Retraction Distance: 3 mm
- Retraction Speed 25.0 mm/s
- Retraction Extra Prime Amount: 0.5 mm ^3
- Additionally, I've enabled the Z hop when retracted setting, "Hopping" at a height of 1 mm.
I'm still seeing some markings on the top layer and some under extrusion on the first layer.
-
07-24-2019, 10:52 AM #2
- Join Date
- Jul 2019
- Posts
- 4
Hey Dude!
Try these settings, They seemed to fix the problems I had.
- Initial Printing Temperature: 210
- Printing Speed - 50 mm/s
- Printing Temperature: 210
- Bed Temperature: 45
- Final Printing Temperature: 190
- Retraction Distance: 4.5 mm
- Retraction Speed 40.0 mm/s
- Retraction Extra Prime Amount: leave alone