    What i have so far:
    print temp: 240c
    bed temp: 80c
    those seem to be spot on. Getting good layer adhesion and it's sticking way way better than it was at 65c.

    retractions wise currently up to 4mm at 70mm/s.

    Just changed from 50mm/s = which is good, but slow. To 60mm/s - still slow, but I want all the speed I can get :-)
    Running at 0.32mm layer with first layer at 150% height.

    Got first layer speed at 10%, I'll try that at 15% for the next test.

    Right think this is good as it's going to get.

    15% first layer
    65mm/s max speed - tempted to go for 75, but everything I've read reckons 65 is about as good as it gets.
    4.5mm retraction at 70mm/s
    240 print temp
    80c bed temp
    fan is on 0% first layer and 50% for all others.
    stringing is minimal. Top klayer finish is acceptable.
    Adhesion on the printbite looks good. no lifting visible anywhere.

    Time to make an actual mould :-)
    Last edited by curious aardvark; 03-27-2019 at 12:22 PM.