actually the thicker the layer, the greater chance of it being watertight. Fewer layers = fewer chances for holes.
Print fairly slowly, no infill (important) and 0.3-0.4 layer thickness.
I have managed to print water tight pet-g vases, so it is doable :-)
With pet-g you want the lower end of the printing range for better layer bonding.