So it works for you - good. It is not everyone's choice. For me it is not worth the expense due to the reports of poor ABS performance.

Glass can compensate for build plate irregularities.

I don't have to put glass in the freezer. PLA will come off almost instantly as will PETG. Having multiple glass plates means I can pull a print still on the glass and add a new glass and ready to go in a minute. This is especially good for ABS where I don't want to force the cooling. I can set the print aside and let it cool slowly to avoid warping or cracking.
I also have glass plates with PEI on them for problem prints.
It gives me options. This is what works and I know how it performs so I use it.



Quote Originally Posted by curious aardvark View Post
gluesticks are good.

why is glass better than printbite ?
i don't need to put it in the freezer, put anything on it or change plates even if I leave it to cool it only takes 10 minutes or so.
I have one surface and no messing about.