10-20-2013, 06:21 PM #1I actually do the opposite. I print with the first layer at 110C and the other layers at 80C within my "garbage chamber" (clear garbage bag chamber). I find that if I set the temp above 100C for the entire print I get some heat distortion of the part on the bottom layers.
Eric
Do you use kapton tape or do you print directly to the glass?