image.jpgimage.jpgimage.jpgimage.jpgimage.jpgHere's a print I did going back to my basic settings.

Print temp - 210 Celsius
bed temp - 70 celsius
print speed - 30mm/s
layer height - 0.2mm
initial layer height - 0.2mm
retraction - 4mm
retraction speed - 30mm/s
infill - 15%
shell width - 0.8mm (0.4mm nozzle)
flow - 100%
makerfarm black PLA
cooling fan enabled on full speed
e-step calibration was good
bed leveling was good
z offset was good

honeslty im just glad I can print objects this cool. But I would like to improve it. Two thoughts I had were that maybe my Hobbed bolt isn't tightened right causing inconsistent extrusion or maybe my PLA has absorbed water because it's hydroscopic. I know I can put the PLA in an oven to dry it out but I don't know how tight my honbed bolt should be. Could someone let me know? And other ideas. Thanks! I really appreciate it.