Close



Results 1 to 8 of 8

Hybrid View

  1. #1
    Engineer
    Join Date
    Oct 2013
    Location
    new jersey
    Posts
    752
    pet is a sticky plastic. if you are getting it collecting on the nozzle then that means you are overextruding. if its only collecting while on the first layer then you are squishing your first layer too much. in anycase, its not necessarily from oozing. any overextruded material will be collected by the nozzle.

  2. #2
    Engineer
    Join Date
    Dec 2014
    Location
    Canada
    Posts
    498
    When I do a cube test calibration and measure the wall thickness its correct. So i feel my extrusion multiplier is accurate