    I used the powder to help release the part as im using a close first layer to prevent curling.

  2. #2
    I just got my heated bed thermistor in the mail and set it up... even a small 25mm test cube is peeling off in the corners at 60c... strange... it actually didnt peel at room temperature (pre heated bed) with PEI (glossy side)
    PS this is with PLA, not even ABS