    He said the packaging listed 210 as the upper limit. It seems high, but I imagine it could work at that temp if it was constantly flowing. However as support material what happens is the PVA will sit there for a minute or 2 each layer and just cook in the nozzle.

  2. #12
    Super Moderator curious aardvark's Avatar
    Join Date
    Jul 2014
    Posts
    8,818
    I've got some pva - somewhere, not got round to trying it yet.