I use PLA and PLA+ 1.75
The lifting occurs more with the pla+.
I might try the hairspray trick.
Thanks
Type: Posts; User: Ouralan
I use PLA and PLA+ 1.75
The lifting occurs more with the pla+.
I might try the hairspray trick.
Thanks
Sometimes my 3D print will come away from the heated bed. The temp is set to 50°CMore often than not, it is with large area projects.Should I be raising the bed temp?
I'm using SketchUp to create the design and then Wanhao (came with my printer) to create the GCODE.
If I design the object with shapes hidden internally, would the shapes get printed (even though...
I will look into that.
I would like to know what method to use in order to make a part of an object solid while the rest is hollow (whatever the fill density is set to).