To keep it simple I'm printing pretty much a cup.

I'm using a Makerfarm 12 Pegasus Basic with an E3Dv6-lite hotend w/ Titan extruder. .40mm nozzle and Slic3r 1.29

I have a glass bed that I clean with denatured alcohol.

I've leveled the bed manually using a spark plug gauge so the the nozzle is 0.23mm from the bed. (I had so close the 1st time I leveled it and blocked the nozzle).

I'm using Hatchbox PLA Nozzle temp is 205c and bed is 105 (it was 75 - 70 range but my room is a little cool at times and I'm getting desperate) this has addressed the part from lifting of the with the brim.

The 1st layer is 0.35mm and 0.2mm for the rest.

Up until recently I was printing fine without brims, I started using brims after I had a larger print that kept curling on the edges, I'm wondering if i should just go back to printing my small stuff with out brims.

The problem is even though I've set the brim to 10, and a Raft 3 layers high it starts to separate at the rafts connection to the model.

I'm unsure what I can do to address this, I willing to try a different slicer (but I question if this really is the problem).

Anybody have any insight they can share?

Thanks