    Troubleshooting TPE w/ Powerspec I3 plus

    New to 3D printing and I could use some advice on what my prints are trying to tell
    me, the following is done is Cura.


    First Print


    • Print speed - 30mm/s
    • Print temp. - 235°
    • Bed temp. - 55°
    • Initial layer thickness - 0.3
    • Initial layer line width - 100

    *Printer set to run it at 35% from there moved up to 55%. No advanced speed changes

    Second Print


    • Print speed - 15mm/s
    • Travel speed - 15 mm/s
    • Bottom layer speed - 15 mm/s (rest of advanced speeds set to 0 to match print speed)
    • Print temp. - 235°
    • Bed temp. - 55°
    • Initial layer thickness - 0.3
    • Initial layer line width - 100

    *Flow increased by 5% (105%) resulted in a slightly better base. Yet still faulted when layering the ends of the dpad.




    Last edited by SmoothVoltron; 02-12-2017 at 01:59 PM.