Hi
I am having a real problem getting all unfused powder out of a porus structure. Have tried up to 6 hours of ultra sonic baths and argon blasting still no joy.

Dose anybody have experience or advice on how to do this.

Printing using Titanium up 0um to 45um on porus structure.

Thanks for the advice.