Really nice looking. Clean and excellent wire/cable management.
Printable View
Really nice looking. Clean and excellent wire/cable management.
Does that drag chain run into the aluminum extrusion at the top?
easy way to reduce 80% of the warping with ABS.. Switch to PETG, it doesnt shrink and warps much less then ABS,
I use PETG and I add a few mouse ears to parts that will likely warp and it fixes the issue.
plus ABS is toxic so avoid using it. PETG isnt toxic and its very strong
I dont use an enclosure yet :)
I am having such a hard time getting petg figured out. for the right extrusion/ temp settings etc. I don't mind the strings but small prints I am wondering if I need a print fan because it is not working, and the first layer seems to have issues sticking, which is really odd as I have a sheet of PEI, However my first print with PETG, I printed at ABS temps, and ran into some issue, and had to pry the print off, which might have messed up the pei, and I am wondering if it warped my glass-cork-wood bed.
for PETG I print 245 nozzle with Fan blowing 100%, 80 bed with PEI, with great results
I have had great success printing PETG at 240C/80C with Garnier Fructis Extreme Hold #5 on glass.
PETG works great for me at 240/80 and elmers kid glustick on my glass.
I am just printing PETG at 230 with no heatbed on painters tape & elmer's gluestick on Mirror from Lowes.