So here's a single layer print. I got distracted while doing this (ooh, shiny object!) and forgot to post the update that I promised. I've got two primary areas of concern - one is the obvious circle on the right side of the print, the other is the area in the center of the left half that looks sloppy.
The right side issue is because there are holes in my print bed where it is bolted to the PCB. The Kapton tape overlays them, but there is an air pocket between the tape and bolt head. Clearly not a good spot to print. I'm going to avoid printing on those in the future. Any suggestions on adding a PLA usable build plate on top of a heated bed? Add a layer of glass with some binder clips maybe?
As for the left half of the print, any ideas? I'll check my last saved g-code to see what temp it ran at. Not at home now, so I'll check that later.
Attachment 3885