3 Attachment(s)
Sputtering, poor base adherance
Ran into some poor print issues last night.
Machine: Ender 5 Plus
Filament: Coex PLA-- JUST OPENED
Nozzle temp: 245° c
Bed temp: 65° c
Never had issues with Coex before. Usually prints with zero issue.
I was immaculate in my leveling and z offset tuning.
Filament would stutter, not forming consistent lines, would not adhere to the buildplate without lots of glue
I wondered if the over abundance of glue caused the spottiness?
Is there a way to adjust the pressure place on the filament in order for it to pass more consistently through the extruder?
Attachment 18282Attachment 18281Attachment 18283