    I'm having problems with the material during a build of 20 hours + can anyone help?

  2. #2
    Super Moderator curious aardvark's Avatar
    Join Date
    Jul 2014
    Posts
    8,818
    not without at least some information :-)

    Remember we're not in your workshop with you - you have to tell us stuff.

    Like: what material, what printer, what settings - oh yeah and what problem :-)

    (quick internet search later)

    so it's an industrial beast with uv cured multijet resin printing. Often used for jewellery making via lost wax process.

    So what's the problem ?
    Last edited by curious aardvark; 10-12-2015 at 10:59 AM.

  3. #3
    Student
    Join Date
    Jun 2014
    Location
    West Horndon, Essex, England
    Posts
    2
    We're using ProCast acrylic. During a large build up to 90mm high it looks as if the support material mixes with the acylic so them we don't get model material we just get wax

  4. #4
    Hello,

    My question to you is are you still having problems if so. you can email me at blakeignoffo@yahoo.com and i can help you resolve pretty much anything with these printers i have been a 3d systems tech for almost four years now with background in projet rev a and b 3000 printers, 3500 and 3510 printers along with a lot of other 3d systems printers.